- - Excellent hardness
- - Excellent acid corrosion resistance
- - Very good alkali corrosion resistance
- - Coating thickness can be built up to 250 microns
Packers, polished rods, tubing products, couplings, threads protection, pump elements, valves, pony rods, sucker rods, manifolds, pup joints, seal surface, rotors, gear boxes, bearings, sand screens, etc.
Phosphorous contents wt% | 11-15% |
Melting Point | 880ºC |
Density | 7.9 g/cm³ |
Hardness | |
As plated | 380-520VHN 100 |
Heat treated | 820-1000 VHN 100 |
Ductility | 1.3% Elongation |
Wear Resistance | see below plated and heat treated |
As plated | 8-10 TWI |
Heat treated | 2-4 TWI |
Magnetic properties | Non- magnetic |
Electrical Resistivity | 35-85 Micron ohm/cm |
Corrosion | Excellent |
Wear Resistance | Very Good |